Behavior of Iron Magnetization and Magnetic Separation During Roasting Cyanide Tailings
发布时间:2024-08-09
点击次数:
- 所属单位:
- 冶金工程学院
- 发表刊物:
- Materials for Renewable Energy & Environment (ICMREE), 2011 International Conference on
- 关键字:
- 中文关键字:尾渣;还原;焙烧;磁性铁;磁选;回收率;,英文关键字:tailings; reduction; roasting; magnetic iron; magn
- 摘要:
- Given the comprehensive utilization problems of tailings in gold smelting, the behavior of iron in the roasting process is discussed in this paper and the optimal conditions are obtained through reduction roasting of the cyanide tailings. The results show that the amount of iron in the cyanide tailings is 35.55%, but the amount of magnetic iron is only 0.28% of all the iron. An iron ore concentrate with iron grade of 52.81% and recovery of only 20.43% can be obtained by high-intensity magnetic separation to the cyanide tailings. After being reduction roasted at the conditions of 750℃,addition volume of pulverized coal 6%,1h and water cooling, the magnetic iron reached up to 84.83%. Have low-intensity magnetic separation on the roasted tailing, the iron grade of the iron ore concentrate is 64.39% and the recovery is 84.67%.
- 备注:
- (会议EI)
- 合写作者:
- 韦武强
- 第一作者:
- 巨建涛,马红周,刘佰龙,张朝晖
- 论文类型:
- 期刊论文
- 卷号:
- 卷:
- 期号:
- 期:
- 页面范围:
- 页:874-877
- 是否译文:
- 否
- 发表时间:
- 2011-05-01
- 上一条:预应力混凝土用钢棒研究现状分析
- 下一条:1种钛铁矿的还原实验研究